Focus on heavy equipment
Most ore drying projects hit the same three snags. Teams size the rotary drum around wrong incoming moisture numbers. Fuel estimates ignore the actual water that needs to evaporate. Wear parts get picked for sand, not tough, abrasive ore. Fix these early at quotation, and you avoid expensive rework later.
Your downstream process sets final moisture, not what the dryer can reach.
| Material | Outlet Moisture | Purpose |
|---|---|---|
| Iron ore concentrate for shipping | 8–10% | Meet transport moisture limits |
| Manganese / chrome ore powder for briquetting | 2–4% | Keep binder strength steady |
| Lithium slag before grinding | 1–2% | Boost mill output, cut dust |
| Petroleum coke for calcination | 1–3% | Keep kiln running smooth |
| Sand for dry mortar | <0.5% | Consistent mixing and bagging |
| Sludge for further treatment | 20–30% | Partial drying for lower cost |
Over-drying wastes fuel. It also raises dust and fire risk. Get the required outlet moisture agreed in writing before sizing. Mines, briquette plants and cement lines all have different standards for “dry enough”.
Example: 1000 t/d ore, 20% inlet moisture, dried to 2%
| Item | Value |
|---|---|
| Dry solids | 800 t/d |
| Finished product | 816 t/d |
| Water to evaporate | 184 t/d ≈7.65 t/h |
A “1000 t/d” dryer rating means nothing without inlet moisture. Same unit:
12% incoming moisture: ~102 t/d water removed
25% incoming moisture: ~235 t/d water removed
Always ask for capacity numbers matched to your real feed moisture.
We size drums by evaporation rate. For mineral ore with inlet gas at 600–800°C:
Standard: 50–80 kg water / m³ drum volume / h
Fine, sticky or heat-sensitive ore: use lower rates
Coarse, free-flow lump ore: use higher rates
Using the example above: 7650 kg/h ÷ 60 kg/(m³·h) ≈128 m³ drum volume. A Φ2.8×21 m drum works. For fine ore, use 50 kg/(m³·h): need ~153 m³, Φ3.2×20 m drum.That explains why two quotes for “1000 t/d” can call for very different drum sizes — one calculated for coarse ore, one for fines.
Direct-fired rotary dryer baseline: 4000 kJ to evaporate 1 kg water. Well-built units hit 3400 kJ/kg. For 184 t of water evaporated daily:
| Fuel Type | Consumption |
|---|---|
| Coal (25 MJ/kg, 85% efficiency) | ~34.6 t/day |
| Natural gas (36 MJ/m³) | ~24000 m³/day |
| Biomass (15 MJ/kg) | ~58 t/day |
Fuel makes up 70–85% of running cost. Two simple ways to cut bills:
1. Cut inlet moisture ahead of drying, with filter presses or stockpile drainage. Drop moisture from 20% to 15%, fuel cost falls roughly 28%.
2. Tap waste heat from kilns, furnaces or on-site generators. Waste heat recovery is the biggest cost saver for mine drying lines.
Lifter flights and wear liners: Hard ore wears plain steel fast. Fit bolt-on replaceable flights and wear-resistant liners. Plan replacement every 6–12 months, based on silica levels.
Dust control: Fine ore creates far more dust than sand. Size your baghouse around fines share, not total throughput.
Sulfide ore overheating: Keep material temperature below 150°C. Hot sulfide ore reacts with air, releases SO₂ and creates strong odour.
Clay-rich feed caking: Ore high in clay sticks and balls up at the drum inlet. Fix this with dry product back-mixing or a lump breaker before feeding.
It depends on the next step: 8–10% for iron ore concentrate shipment; 2–4% for briquetting; 1–2% before grinding; under 0.5% for dry mortar sand. Confirm with your downstream team first.
For ore going from 20% to 2% moisture: roughly 30–40 kg coal per ton of wet feed, or ~24000 m³ gas for 1000 t/d feed. Fuel use moves up and down with water load, so always check against your inlet moisture.
Yes. But fine ore at 25% moisture needs a larger drum, higher inlet heat, and carries higher sticking risk. If feed stays above 25% moisture, mechanical dewatering before drying usually saves more money.
Most ore drying projects hit the same three snags. Teams size the rotary drum around wrong incoming moisture numbers. Fuel estimates ignore the actual water that needs to evaporate. Wear parts get picked for sand, not tough, abrasive ore. Fix these early
Heat source choice matters for quartz sand drying. It affects sand quality, running cost and environmental compliance. We compare three common heat sources here.
Pond ash deposited in ash ponds carries high moisture. It is sticky and tends to form hard lumps. Raw pond ash cannot be used directly as construction raw material. Stockpiling also takes up land and brings dust pollution. A proper drying system turns thi
The petcoke drying production line, delivered by our company, has successfully completed all commissioning phases and is now in full operation in Yicheng, Hubei. This system addresses a critical dehydration stage for the client’s petcoke deep-processing o